PRODUCT NO. Category Trade Name
Barlog Plastics KEBAFORM C 6027 POM Copolymer, 30% mineral reinforced Acetal Copolymer, Mineral Filled KEBAFORM
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced Acetal Copolymer, Mineral Filled KEBAFORM