BASF Ultramid® 1000-11 NF2001 PA66 (Conditioned) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® 1000-2 NF2001 PA66 (Conditioned) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® 1310-11 NF2001 PA66 (Conditioned) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® 1310-11 NF2001 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® 1403-2 BK ND3007 PA66 (Conditioned) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Conditioned) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 66 H2 G/25-V0KB1 NAT 0046 PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 66 H2 G/35-V0KB NAT 0046 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Conditioned) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A24 E 01 PA66 |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A27 E 01 PA66 (Conditioned) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A27 E 01 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A27 E PA66 |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A27 EZ 01 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A34 01 PA66 (Conditioned) |
Nylon 66, Unreinforced, Flame Retardant |
Ultramid®
|
BASF Ultramid® A34 01 PA66 (Dry) |
Nylon 66, Unreinforced, Flame Retardant |
Ultramid®
|
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3G5 25% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3G5 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Dry) |
Nylon 66, 10% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG3 PA66 (Conditioned) |
Nylon 66, 20% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG3 PA66 (Dry) |
Nylon 66, 20% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG5 BK00564 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG7 35% Glass Filled PA66 (Conditioned) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG7 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG7 BK 00564 35% Glass Filled PA66 (Conditioned) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3HG7 BK 00564 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3K BK00464 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3K PA66 (Conditioned) |
Nylon 66, Unreinforced, Flame Retardant |
Ultramid®
|
BASF Ultramid® A3K PA66 (Dry) |
Nylon 66, Unreinforced, Flame Retardant |
Ultramid®
|
BASF Ultramid® A3K Q601 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3K Q603 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3L HP BK20465 PA66 (Conditioned) |
Nylon 66, Impact Grade |
Ultramid®
|
BASF Ultramid® A3L HP BK20465 PA66 (Dry) |
Nylon 66, Impact Grade |
Ultramid®
|
BASF Ultramid® A3L HP PA66 (Dry) |
Nylon 66, Impact Grade |
Ultramid®
|
BASF Ultramid® A3L HP UV BK 23220 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3UG5 BK 23260 25% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3UG5 BK 23260 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3W BK 00464 PA66 (Conditioned) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3W BK00464 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3W PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3W Q601 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Conditioned) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3W2G6 BK 20560 30% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3W2G6 BK 20560 30% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG10 50% Glass Filled PA66 (Conditioned) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG10 50% Glass Filled PA66 (Dry) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG10 BK00564 50% Glass Filled PA66 (Dry) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Conditioned) |
Nylon 66, 20% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Conditioned) |
Nylon 66, 20% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG3 BK 00564 15% Glass Filled PA66 (Dry) |
Nylon 66, 20% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG5 BK00564 25% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 BK00564 30% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 HRX BK 23591 30% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 HRX BK 23591 30% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 LS BK 23189 30% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG6 LS BK 23189 30% Glass Filled PA66 (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG7 BK00564 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG7 BK23210 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG7 HP BK 20560 35% Glass Filled PA66 (Conditioned) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG7 HP BK 20560 35% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WG8 BK 20560 40% Glass Filled PA66 (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3WGM53 BK20560 25/15% Glass/Mineral Filled PA66 (Conditioned) |
Nylon 66, Glass/Mineral Filled |
Ultramid®
|
BASF Ultramid® A3WGM53 BK20560 25/15% Glass/Mineral Filled PA66 (Dry) |
Nylon 66, Glass/Mineral Filled |
Ultramid®
|
BASF Ultramid® A3X2G10 BK 23187 50% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X2G10 BK 23187 50% Glass Filled PA66 FR (Dry) |
Nylon 66, 50% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Conditioned) |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Ultramid®
|
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry) |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Ultramid®
|
BASF Ultramid® A3X2G5 BK 23185 25% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X2G5 BK23187 25% Glass Filled PA66 (Dry) |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Ultramid®
|
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Dry) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X3G5 25% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X3G5 25% Glass Filled PA66 FR (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X3G5 BK 23187 25% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X3G5 BK 23187 25% Glass Filled PA66 FR (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X4G7 35% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3X4G7 BK 23079 35% Glass Filled PA66 FR (Conditioned) |
Nylon 66, 40% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Dry) |
Nylon 66, 30% Glass Fiber Filled |
Ultramid®
|
BASF Ultramid® A3Z BK 30464 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3Z HP BK 20465 PA66 (Dry) |
Nylon 66, Unreinforced |
Ultramid®
|
BASF Ultramid® A3Z HP BK20465 PA66 (Dry) |
Nylon 66, Impact Grade |
Ultramid®
|