Polymer Property : Volume Resistivity = 5.50e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 5.50e+12 ohm-cm

@Temperature 70.0 °C
5.50e+12 ohm-cm

@Temperature 158 °F
IEC 60502
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Volume Resistivity 5.50e+12 ohm-cm

@Temperature 70.0 °C
5.50e+12 ohm-cm

@Temperature 158 °F
IEC 60502
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Volume Resistivity 5.50e+12 ohm-cm

@Temperature 70.0 °C
5.50e+12 ohm-cm

@Temperature 158 °F
ASTM D257
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho..
Volume Resistivity 5.50e+12 ohm-cm

@Temperature 70.0 °C
5.50e+12 ohm-cm

@Temperature 158 °F
ASTM D257
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with..
Volume Resistivity 5.50e+12 ohm-cm

@Temperature 70.0 °C
5.50e+12 ohm-cm

@Temperature 158 °F
IEC 60502
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..