Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE) Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE) Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidan® EC/MD Polyethylene, Crosslinked (XLPE) Medium density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards complying.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/220 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/400 Thermoset Elastomer (TSE) Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method).Standards complying: Cenelec H.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Si.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/440 Thermoset Elastomer (TSE) Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method)Standards complying: Cenelec HD.. |
|||
Volume Resistivity | 4.10e+15 ohm-cm @Temperature 20.0 °C |
4.10e+15 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/450 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |