Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+13 ohm-cm @Temperature 60.0 °C |
3.00e+13 ohm-cm @Temperature 140 °F |
JIS-K-6723 |
Denka VINYKON W4200 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 3.00e+13 ohm-cm @Temperature 30.0 °C |
3.00e+13 ohm-cm @Temperature 86.0 °F |
JIS-K-6723 |
Denka VINYKON W4800 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 3.00e+13 ohm-cm @Temperature 60.0 °C |
3.00e+13 ohm-cm @Temperature 140 °F |
JIS-K-6723 |
Denka VINYKON W5230 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |