Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 2.00e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm

@Temperature 60.0 °C
2.00e+13 ohm-cm

@Temperature 140 °F
JIS-K-6723
Denka VINYKON W1021 PVC, W grade for insulation, for sheaths
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Volume Resistivity 2.00e+13 ohm-cm

@Temperature 60.0 °C
2.00e+13 ohm-cm

@Temperature 140 °F
JIS-K-6723
Denka VINYKON W1022 PVC, W grade for insulation, for sheaths
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Volume Resistivity 2.00e+13 ohm-cm

@Temperature 30.0 °C
2.00e+13 ohm-cm

@Temperature 86.0 °F
JIS-K-6723
Denka VINYKON W3050 PVC, W grade for equipment cords, for heat resistance
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Volume Resistivity 2.00e+13 ohm-cm

@Temperature 100 °C
2.00e+13 ohm-cm

@Temperature 212 °F
IEC 672-1
CeramTec 614/698 Alumina, 96%
614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.