Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 100 ohm-cm @Temperature 23.0 °C |
100 ohm-cm @Temperature 73.4 °F |
ASTM D991 |
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables LE0515 is an easy strippable crosslinkable semi conductive insulation shield compound designed for medium voltage (5kV-46kV) power cable applications. Application: LE0515 is especially suitable for.. |
|||
Volume Resistivity | 100 ohm-cm @Temperature 90.0 °C |
100 ohm-cm @Temperature 194 °F |
ASTM D991 |
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables LE0515 is an easy strippable crosslinkable semi conductive insulation shield compound designed for medium voltage (5kV-46kV) power cable applications. Application: LE0515 is especially suitable for.. |
|||
Volume Resistivity | 100 ohm-cm @Temperature 23.0 °C |
100 ohm-cm @Temperature 73.4 °F |
ASTM D991 |
Borealis LE0315 Polyethylene Compound, Crosslinkable, Semiconductive LE0315 is an Easy Strippable Semi conductive Insulation Shield for EPR Insulated, Medium Voltage (5-46 kV) Cables. Strip forces range from 5 to 10 lbs/0.5". Specifications: LE0315 meets the applica.. |
|||
Volume Resistivity | 100 ohm-cm @Temperature 90.0 °C |
100 ohm-cm @Temperature 194 °F |
ASTM D991 |
Borealis LE0315 Polyethylene Compound, Crosslinkable, Semiconductive LE0315 is an Easy Strippable Semi conductive Insulation Shield for EPR Insulated, Medium Voltage (5-46 kV) Cables. Strip forces range from 5 to 10 lbs/0.5". Specifications: LE0315 meets the applica.. |
|||
Volume Resistivity | 100 ohm-cm @Temperature 23.0 °C |
100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis LE0511 Polyethylene Compound, Crosslinkable, Semiconductive LE0511 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0511 is intended for strippable outer semi conductive s.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis LE0516 Polyethylene Compound, Crosslinkable, Semiconductive LE0516 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0516 is intended for strippable outer semi conductive s.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis LE0574 Polyethylene LE0574 is a thermoplastic black polyethylene compound, specially designed for strippable semi conductive screen applications. It can be used in thermoplastic form or crosslinked via a grafting proce.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis LE0592 Polyethylene LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE m.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis Supersmooth™ LE0550 Polyethylene Insulation Compound, Crosslinkable Supersmooth™ LE0550 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE0550 is intended for semiconduct.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis Supersmooth™ LE0592S Polyethylene Supersmooth™ LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Supersmooth™ LE0592S is intended for semiconductive applicat.. |
|||
Volume Resistivity | >= 100 ohm-cm @Temperature 400 °C |
>= 100 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
Volume Resistivity | 100 ohm-cm @Temperature 400 °C |
100 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Volume Resistivity | 100 ohm-cm @Temperature 400 °C |
100 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDP.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Trelleborg Horda Cable E7310 Bonded Insulation Shielding And Conductor Screen E7310 is a silane crosslinkable semiconductive compound for medium voltage cables. The material is designed as a conductor screen and bonded insulation shielding.E7310 meets the requirements as bel.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
DC; ISO 3915 |
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage.. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
DC; ISO 3915 |
Borealis LE7710 Polyethylene Compound, Semiconductive, Thermoplastic LE7710 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7710 is intended for semiconductive applications in medium voltage .. |
|||
Volume Resistivity | <= 100 ohm-cm @Temperature 23.0 °C |
<= 100 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis Supersmooth™ LE8280 Polyethylene Insulation Compound, Crosslinkable Supersmooth™ LE8280 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE8280 is intended for semiconduct.. |