Electrical Properties Metric English Comments
Volume Resistivity 9.70e+14 ohm-cm
9.70e+14 ohm-cm
ASTM D257
Teknor Apex HFFR 2005 Polyolefin, Halogen Free
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable JacketingAgency Ratings: IEC Unsp..