Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.30e+14 ohm-cm | 8.30e+14 ohm-cm | |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Volume Resistivity | 8.30e+14 ohm-cm | 8.30e+14 ohm-cm | |
Resinlab® EP750 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP750 Clear is a two part unfilled epoxy structural adhesive which ingredients are listed in the Code of Federal Regulations Title 21 175.105 (Adhesives) and 175.300 (Resinous and polymer.. |