Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 75 ohm-cm | 75 ohm-cm | IEC 93 |
Nilit FRIANYL A63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Volume Resistivity | 75 ohm-cm @Time 540 sec |
75 ohm-cm @Time 0.150 hour |
18% Carbon Black |
TIMCAL ENSACO™ 260G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Volume Resistivity | 75 ohm-cm | 75 ohm-cm | ASTM D257 |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |