Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.70e+17 ohm-cm | 6.70e+17 ohm-cm | DIN 53 482, VDE 0303, Part 3 |
Hippe PEI A material with very high mechanical strength and high thermoforming stability which can be used at high temperatures. Distinguished by constant dielectric properties, a wide range of frequency and .. |