Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.50e+15 ohm-cm | 6.50e+15 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Volume Resistivity | 6.50e+15 ohm-cm | 6.50e+15 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Volume Resistivity | 6.50e+15 ohm-cm | 6.50e+15 ohm-cm | |
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and .. |