Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Temperature 23.0 °C |
5.50e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Volume Resistivity | >= 5.50e+16 ohm-cm | >= 5.50e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Volume Resistivity | >= 5.50e+16 ohm-cm | >= 5.50e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm | 5.50e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Thickness 3.00 mm |
5.50e+16 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Volume Resistivity | 5.50e+16 ohm-cm @Thickness 3.00 mm |
5.50e+16 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |