Polymer Property : Volume Resistivity = 5.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity >= 5.00e+16 ohm-cm
>= 5.00e+16 ohm-cm
ISO.167 DN.53482
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Volume Resistivity >= 5.00e+16 ohm-cm
>= 5.00e+16 ohm-cm
ISO.167 DN.53482
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom..
Volume Resistivity >= 5.00e+16 ohm-cm
>= 5.00e+16 ohm-cm
ISO.167 DN.53482
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P..
Volume Resistivity >= 5.00e+16 ohm-cm
>= 5.00e+16 ohm-cm
ISO.167 DN.53482
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500
PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or ..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)  (Unverified Data**)
Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)  (discontinued **)
Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
Manifattura Cattaneo PVDF
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 120H PC/ABS alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 210 PC/ABS alloy
Characteristics:Impact resistantHeat resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grillA..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 215 PC/ABS alloy
Characteristics:Dimensional stabilityHigh heat resistanceGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl ..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 220 Polymer Alloy, High Impact
Excellent impact, formability and weather resistance.220 is a high impact grade.Applications: Automotive instrument panels and knob typesInformation provided by Samyang.
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 225 PC/ABS alloy
Characteristics:Impact resistantHeat resistantDimensional stabilityApplications:Air con. grillAll information provided by Samyang
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Standard
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
Polyplastics Duranex® 2002U Polybutylene Terephthalate (PBT), Weather resistance
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 60093
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 93
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
IEC 93
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Volume Resistivity 5.00e+16 ohm-cm

@Temperature 22.8 °C
5.00e+16 ohm-cm

@Temperature 73.0 °F
ASTM D257
Ensinger TECASON™ S Polysulfone (PSU)
TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD..
Volume Resistivity >= 5.00e+16 ohm-cm
>= 5.00e+16 ohm-cm
ISO.167 DN.53482
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 200 PC/ABS alloy
General purposeCharacteristics:Impact resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grill..
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant
Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang