Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+10 ohm-cm | 5.00e+10 ohm-cm | |
Industrial Laminates/Norplex MC511A Glass Fabric Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar.. |
|||
Volume Resistivity | >= 5.00e+10 ohm-cm @Temperature 20.0 °C |
>= 5.00e+10 ohm-cm @Temperature 68.0 °F |
|
Sibur O-40 Compound 239 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | >= 5.00e+10 ohm-cm @Temperature 20.0 °C |
>= 5.00e+10 ohm-cm @Temperature 68.0 °F |
|
Sibur O-40 Compound OM-40 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | 5.00e+10 ohm-cm @Temperature 50.0 °C |
5.00e+10 ohm-cm @Temperature 122 °F |
ASTM D257 |
Teknor Apex APEX® 80-C118Q Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Volume Resistivity | 5.00e+10 ohm-cm | 5.00e+10 ohm-cm | |
Covestro Texin® 950 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated f.. |