Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.90e+17 ohm-cm | 4.90e+17 ohm-cm | 50% RH and at 90% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Volume Resistivity | 4.90e+17 ohm-cm | 4.90e+17 ohm-cm | 50% RH and at 90% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Volume Resistivity | 4.90e+17 ohm-cm | 4.90e+17 ohm-cm | 50% RH and at 90% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |