Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 300000 ohm-cm | 300000 ohm-cm | |
Shinil Chemical SHINCON PEI-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Volume Resistivity | 300000 ohm-cm | 300000 ohm-cm | |
Shinil Chemical SHINCON PES Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |