Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 3.60e+15 ohm-cm | <= 3.60e+15 ohm-cm | |
Cytec (Conap) FR-2000 / FR-200 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 3.60e+15 ohm-cm | 3.60e+15 ohm-cm | |
Dow Corning 3-4680 SILICONE GEL KIT Two-part, transparent blue, fast RT or heat cure, low viscosity.Information provided by Dow Corning |