Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.20e+16 ohm-cm | 3.20e+16 ohm-cm | ASTM D257 |
Owens Corning Glass Fiber Reinforced Polyester (PBT), 30 wt.% glass Thermoplastic Polyesters are resistant to most organic solvents, weak acids and alkalis. They are not recommended with strong acids and alkalis or for prolonged use in hot water. Data provided by t.. |
|||
Volume Resistivity | >= 3.20e+16 ohm-cm | >= 3.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Volume Resistivity | >= 3.20e+16 ohm-cm | >= 3.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Volume Resistivity | >= 3.20e+16 ohm-cm | >= 3.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
Volume Resistivity | >= 3.20e+16 ohm-cm | >= 3.20e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific) 30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | >= 3.20e+16 ohm-cm | >= 3.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Volume Resistivity | >= 3.20e+16 ohm-cm | >= 3.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |