Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+8 ohm-cm | 3.00e+8 ohm-cm | |
Pyrotek TS-106 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan / Red color. High heat resistance. UL recognized.Information provided by Pyrotek. |
|||
Volume Resistivity | 3.00e+8 ohm-cm | 3.00e+8 ohm-cm | |
Pyrotek TS-207 Thermoset Electrical Insulation Product Polymer reinforcement, Polyester resin, Grey color. High strength and good electrical resistance.Information provided by Pyrotek. |
|||
Volume Resistivity | 3.00e+8 ohm-cm | 3.00e+8 ohm-cm | |
Pyrotek TS-235 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek. |