Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 410 PC/PET alloy
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | measured 1 min. after applying DC 500 V; JIS K-6911 |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM 2300R PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ajedium™ Films -- Udel® PSU P-1700 NT-11 Polysulfone (PSU) Udel® P-1700 polysulfones are tough, high-strength thermoplastics that are suitable for continuous use up to 300°F (149°C). Udel Film is resistant to oxidation and hydrolysis and withstand .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP E GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled, Heat Stabilized and High Viscosit.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF10 CBA 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: FoamableAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF15 RD 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: RedTPCI# 862111Information provided by TP Composites,.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | >= 3.00e+16 ohm-cm | >= 3.00e+16 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 615 MD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid MDPEInformation provided by Fainplast Compounds.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | |
Dow Corning SE 4446 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility.Information provided by Dow Corning |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | |
Asahi Glass AFLAS® 100S TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 450N Polymer Alloy, Blow Molding Excellent impact, formability and weather resistance.450N is a blow molding grade.Applications: ConnectorsInformation provided by Samyang. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® S460G15 Polymer Alloy, Reinforced Excellent impact, formability and weather resistance.220 is a reinforced grade.Applications: LCD Panel Frame - for dimensional stabilityInformation provided by Samyang. |
|||
Volume Resistivity | 3.00e+16 ohm-cm @Temperature 23.0 °C |
3.00e+16 ohm-cm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |