Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | ASTM D 257 |
Karina Karintox 70 Polyolefin Compound Halogen free, fire retardant, low smoke and fume polyolefinic compound. Recommended for insulation of electrical cables up to 1KV.Information provided by Karina Indústria e Comércio de Plá.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | |
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | ASTM D 257 |
Karina E 105440-35/1-Y-IS-SD-LM Ivory PVC Compound Heavy metal free PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°CInformation provided by Karina Indús.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | NBR 5403 |
Karina 70900-35/1-E-AC Ivory PVC Compound Flame retardant PVC compound, class 70C (PVC/A), recommended for insulation of electrical wires and cables (BWF).Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInf.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 CC20 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Calcium Carbonate Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 CM16 HS BK 16% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 16% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 CM25 HS BK 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF10 IM L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF12 TL20 12% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 12% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated and Heat Stabiliz.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Volume Resistivity | <= 3.00e+14 ohm-cm | <= 3.00e+14 ohm-cm | |
Cytec (Conap) RN-1000 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FK 90/1 Flexible PVC, Insulation Lead Free Oil resistant insulation |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FKA 92 Flexible PVC, Flame Retardant Insulation Lead Free General purposes |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-20Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 940-07Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wr.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave Design/Construction:Cross Section Type: TriangularArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW201Xxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW601Xxx-P1 0.060" (1.52 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-15Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 89 Flexible PVC, Flame Retardant Insulation Power cables |