Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-20Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape
(discontinued **) Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | ASTM D 257 |
Karina Karintox 70 Polyolefin Compound Halogen free, fire retardant, low smoke and fume polyolefinic compound. Recommended for insulation of electrical cables up to 1KV.Information provided by Karina Indústria e Comércio de Plá.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | NBR 5403 |
Karina 70900-35/1-E-AC Ivory PVC Compound Flame retardant PVC compound, class 70C (PVC/A), recommended for insulation of electrical wires and cables (BWF).Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInf.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 CM25 HS BK 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF10 L 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF6 HS BK 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance:.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF6 L BK 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Volume Resistivity | <= 3.00e+14 ohm-cm | <= 3.00e+14 ohm-cm | |
Cytec (Conap) RN-1000 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FK 90/1 Flexible PVC, Insulation Lead Free Oil resistant insulation |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FKA 85 Flexible PVC, Flame Retardant Insulation Lead Free Power cables |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FKA 92 Flexible PVC, Flame Retardant Insulation Lead Free General purposes |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 23.0 °C |
3.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FRT 91 Flexible PVC, Insulation Telephone cables |
|||
Volume Resistivity | 3.00e+14 ohm-cm | 3.00e+14 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 912-10R12-P1 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularRoll Length: 12 Yards Width, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-05Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-07Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-20Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW202Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW301Rxx-P1 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon LW601Xxx-P1 0.060" (1.52 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 920-15Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Volume Resistivity | >= 3.00e+14 ohm-cm | >= 3.00e+14 ohm-cm | |
Arlon 940-10Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Volume Resistivity | 3.00e+14 ohm-cm @Temperature 20.0 °C |
3.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |