Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.30e+12 ohm-cm | 2.30e+12 ohm-cm | 60°C for 500 hrs |
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Volume Resistivity | 2.30e+12 ohm-cm | 2.30e+12 ohm-cm | ASTM D247 |
Plenco 2311 Phenolic, Granular, Compression Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Volume Resistivity | 2.30e+12 ohm-cm | 2.30e+12 ohm-cm | ASTM D247 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Volume Resistivity | 2.30e+12 ohm-cm | 2.30e+12 ohm-cm | |
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially .. |