Polymer Property : Volume Resistivity = 2.10e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.10e+14 ohm-cm

@Temperature 70.0 °C
2.10e+14 ohm-cm

@Temperature 158 °F
7 days water immersion; IEC 60167
Lucobit Lucofin® 7440 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Volume Resistivity 2.10e+14 ohm-cm
2.10e+14 ohm-cm
IEC 60093
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound
Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak..
Volume Resistivity 2.10e+14 ohm-cm
2.10e+14 ohm-cm
Dow Corning JCR 6140
Two-part, transparent, medium modulus LED encapsulant with high transparency and medium viscosity.Information provided by Dow Corning
Volume Resistivity <= 2.10e+14 ohm-cm
<= 2.10e+14 ohm-cm
Cytec (Conap) FR-1610 / EA-039 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Volume Resistivity <= 2.10e+14 ohm-cm
<= 2.10e+14 ohm-cm
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..