Polymer Property : Volume Resistivity = 1.60e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+17 ohm-cm
1.60e+17 ohm-cm
ASTM D257
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications.
Volume Resistivity 1.60e+17 ohm-cm
1.60e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Volume Resistivity 1.60e+17 ohm-cm
1.60e+17 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL V095 PPE+HIPS (Asia Pacific)
83dc HDT, V0@1.5mm,Higher flow version of PX1007
Volume Resistivity 1.60e+17 ohm-cm
1.60e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Volume Resistivity 1.60e+17 ohm-cm
1.60e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..