Polymer Property : Volume Resistivity = 1.30e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
70°C for 1,000 hrs; JIS-K-6249
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by..
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene
Features:Halogenated Forms:PelletsInformation provided by Multibase
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D 257
SABIC Innovative Plastics Valox® 735 PBT
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re..
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific)
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 735 PBT+PET
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D247
Plenco 1508 Polyester, Briquette, Transfer Molded
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl..
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate..
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
Cured property; ASTM D257
Aptek 2205 A/B Low modulus urethane stacking compound
APTEK 2205-A/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although..
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
3M 7957MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
3M 9057MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..