Polymer Property : Volume Resistivity = 1.30e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
ASTM D257
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer
Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and..
Volume Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
60°C for 500 hrs
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Volume Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
ASTM D257
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global)
Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig..
Volume Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
Tra-Con Tra-Bond Ablebond 481-20 B-Stageable Epoxy Adhesive
Ablebond 481-20 flexible epoxy adhesive is a modification of Ablebond 481-19 adhesive. This adhesive is designed to absorb stresses between adherends with mismatched coefficients of thermal expansio..
Volume Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
ASTM D257
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser..
Volume Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
C96/35/90; IPC TM-650 2.5.17.1
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg
45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c..