Polymer Property : Volume Resistivity = 0.0034 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.0034 ohm-cm
0.0034 ohm-cm
cured 1 hr @ 110°C
Tra-Con Tra-Duct 2916 Room Temperature Conductive Silver Epoxy Adhesive
TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good ele..