Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.00090 ohm-cm | 0.00090 ohm-cm | cured 2 min @ 150°C |
Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy TRA-DUCT 2960 is a one or two-part, specially refined and processed silver filled adhesive for high speed manufacturing. Recommended for the microelectronic, automotive computer and telecommunicatio.. |
|||
Volume Resistivity | 0.00090 ohm-cm | 0.00090 ohm-cm | cured 2 hrs @ 65°C |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Volume Resistivity | 0.00090 ohm-cm | 0.00090 ohm-cm | cured 2 hrs @ 65°C |
Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Volume Resistivity | <= 0.00090 ohm-cm | <= 0.00090 ohm-cm | |
Epoxy Technology EPO-TEK® EM127 Electrically Conductive Epoxy Product Description: EPO-TEK® EM127 is a single component, heat curable, electrically conductive epoxy adhesive for semiconductor IC and LED die attach applications.Advantages & Application Notes: .. |
|||
Volume Resistivity | <= 0.00090 ohm-cm | <= 0.00090 ohm-cm | |
Epoxy Technology EPO-TEK® H81A Epoxy Material Description: A two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Information Provided by Epoxy Technolo.. |
|||
Volume Resistivity | <= 0.00090 ohm-cm | <= 0.00090 ohm-cm | |
Atom Adhesives AA-BOND G298 Epoxy Adhesive AA-BOND G298 is a two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Appearance: Resin: Brown, Hardener: Dark Bro.. |
|||
Volume Resistivity | 0.00090 ohm-cm | 0.00090 ohm-cm | Cured: 96 hours at 25°C |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |