Polymer Property : Volume Resistivity = 0.00030 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 60 minutes at 125°C
Resin Technology Group TIGA 901 Room Temperature Curing Silver Conductive Epoxy
100 parts resin to 6 parts hardener. Cure 24 hours at 25°C, 1-4 hours at 65°C, 30-60 minutes at 125°C, or 30 minutes at 150°C.TIGA 901 is an electrically conductive, silver filled epoxy adhesiv..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 30 minutes at 150°C
Resin Technology Group TIGA 908 Gold Bonder - Low Stress Silver Conductive
100 parts resin to 6 parts hardener.TIGA 908 is a low stress, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications which require bonding to gol..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
Gwent Electronic Materials C2010903D2 Curable Silver Range
This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive adhesive that combines good adhesion with excellent electrical properties..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive
TRA-BOND 293-14 silver-filled, electrically conductive epoxy adhesive is designed to provide strong bonds to difficult-to-bond metals, such as nickel, copper, gold and solder. The stress-absorbing c..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 10 min @ 100°C
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive
TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 5 min @ 125°C
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive
TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications ..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
Tra-Con Tra-Duct 2979 Microelectronic Conductive Epoxy Adhesive
TRA-DUCT 2979 is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid t..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive
TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid..
Volume Resistivity 0.00030 ohm-cm

@Temperature 150 °C
0.00030 ohm-cm

@Temperature 302 °F
Tra-Con Tra-Duct 8205 One-Part Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 8205 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of excellent mechanical and electrical..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 5 min @ 160°C
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive
TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop..
Volume Resistivity >= 0.00030 ohm-cm
>= 0.00030 ohm-cm
Epoxy Technology EPO-TEK® E2036 Epoxy
Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o..
Volume Resistivity <= 0.00030 ohm-cm
<= 0.00030 ohm-cm
cured
Atom Adhesives AA-DUCT 2924 Epoxy Adhesive
AA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage; low resistivity bonding applications where good electrical and physical properties over a wide temperature..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o..
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured 1 hr @ 65°C
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive
Information provided by Tra-Con Inc.
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
Cured: 1 hour at 60°C
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit..