Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.00010 ohm-cm | 0.00010 ohm-cm | Conductive Layer |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Volume Resistivity | 0.00010 ohm-cm | 0.00010 ohm-cm | cured 1 hr @ 110°C |
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste s.. |
|||
Volume Resistivity | 0.00010 ohm-cm | 0.00010 ohm-cm | cured 72 hrs @ 25°C |
Tra-Con Tra-Duct 2956 Low Ion Snap Cure Silver Epoxy Adhesive TRA-DUCT 2956 is recommended for the bonding and sealing of electronic components where a combination of electrical and mechanical properties are required. This two-part, smooth, paste system of sil.. |
|||
Volume Resistivity | <= 0.00010 ohm-cm | <= 0.00010 ohm-cm | |
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di.. |
|||
Volume Resistivity | <= 0.00010 ohm-cm | <= 0.00010 ohm-cm | Cured |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Volume Resistivity | <= 0.00010 ohm-cm | <= 0.00010 ohm-cm | |
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value .. |
|||
Volume Resistivity | <= 0.00010 ohm-cm | <= 0.00010 ohm-cm | cured |
Atom Adhesives AA-DUCT 916 Epoxy Adhesive AA-DUCT 916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good elect.. |