Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.3 kV/mm | 845 kV/in | |
Saint-Gobain CHR® SG05-06(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Strength | 33.3 kV/mm | 845 kV/in | |
Saint-Gobain CHR® SG06-06(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Strength | 33.3 kV/mm | 845 kV/in | ASTM D149 |
Arlon 47571R012 0.012" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEThis data represents typical values for the produ.. |