Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 33.1 kV/mm | >= 840 kV/in | At 40 mils; ASTM D149 |
Borealis Polycure™ PC780 Flame Retardant Crosslinking Polyethylene Compound for Low Voltage Insulation Polycure PC780 is a natural, chemically crosslinking polyethylene compound designed for flame retardant low voltage wire insulation and jacketing. PC780 contains a halogen-based, flame retardant ad.. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
Arlon 915-10R##-P2 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Certified to meet all requirements of US Military Specification A-A5.. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
Arlon 912-10X##-P0 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 12 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
Arlon 915-10R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
Arlon 915-15X##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 15 mil thick, Gray, Rectangular cross-section, Self.. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
Arlon 915-10R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |
|||
Dielectric Strength | 33.1 kV/mm | 840 kV/in | ASTM D149 |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |