Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.0 kV/mm | 838 kV/in | ASTM D149 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.50 mm |
838 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | |
Styrolution NOVODUR® P3H-AT ABS, Injection Grade Injection molding grade, antistatic, high gloss, improved chemical and dynamic resistance.Applications: Housings for telephones and household appliances. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A1030SR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-2H black PA*-GF20 Product description: Grivory GV-2H is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | 50%RH; IEC 60243-1 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-4H PA*-GF40 Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40 Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30 Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BZ 1 PA6 Information provided by EMS Grivory |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | ASTM D149 |
PolyOne Geon™ Vinyl Wire & Cable W2300 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |