Polymer Property : Dielectric Strength = 699 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM 2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM 2100F PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing, WRAS certification in recognized colors..
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Ultem 2100N PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Ultem 2100N PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM 2100R PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Dielectric Strength 27.5 kV/mm

@Thickness 1.60 mm
699 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.