Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.3 kV/mm | 667 kV/in | |
Saint-Gobain CHR® 2975-8R Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Dielectric Strength | 26.3 kV/mm | 667 kV/in | ASTM D149 |
Arlon 940-15R##-P0 0.040" (1.02 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 40 mil thick, Red, Rectangular cross-section, Self-f.. |
|||
Dielectric Strength | 26.3 kV/mm | 667 kV/in | ASTM D149 |
Arlon 44576R009A 0.0058" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma.. |