Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 65.59 kV/mm | 1666 kV/in | |
Saint-Gobain CHR® M797 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 65.59 kV/mm | 1666 kV/in | |
Saint-Gobain CHR® M803 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 65.59 kV/mm | 1666 kV/in | |
Saint-Gobain CHR® M815 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 65.59 kV/mm | 1666 kV/in | |
Saint-Gobain CHR® M827 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 65.59 kV/mm | 1666 kV/in | |
Saint-Gobain CHR® M897 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Strength | 65.59 kV/mm | 1666 kV/in | |
Saint-Gobain CHR® K100 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |