Polymer Property : Dielectric Strength = 630 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded  
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d..
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film
Dielectric Strength 24.8 kV/mm
630 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PEI GF30 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Dielectric Strength 24.8 kV/mm
630 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® PEI GF30 TL15 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Dielectric Strength 24.8 kV/mm

@Thickness 1.59 mm
630 kV/in

@Thickness 0.0625 in
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Dielectric Strength 24.8 kV/mm
630 kV/in
In Oil; ASTM D149
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product..
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should..
Dielectric Strength 24.8 kV/mm
630 kV/in
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Dielectric Strength 24.8 kV/mm

@Thickness 3.20 mm
630 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL EN185 PPE+PS
Extrusion grade. Excellent impact strength. 185F (85C) DTUL. UL94 V-1 rated.