Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 24.2 kV/mm | 615 kV/in | |
Dow Corning HV 1540/20P BASE AND CLEAR CURING AGENT 32 Shore, very low viscosity, castable hydrophobic silicone rubber with high tear strength and low temperature cure.Information provided by Dow Corning |
|||
Dielectric Strength | 24.2 kV/mm | 615 kV/in | |
Saint-Gobain CHR® 2916-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°F .. |