Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.1 kV/mm | 536 kV/in | |
Resin Technology Group KONA 870FT-FR Fire Retardant Epoxy Casting System Mix ratio 100 to 4 by weight.KONA 870 FTFR with HARDENER #9 is a versatile epoxy casting system that exhibits unusually high thermal conductivity and low thermal expansion. It is recommended for ele.. |
|||
Dielectric Strength | 21.1 kV/mm | 536 kV/in | 60Hz, Short Time, wet; ASTM D149 |
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B.. |
|||
Dielectric Strength | 21.1 kV/mm | 536 kV/in | ASTM D149 |
Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 11523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |