Electrical Properties Metric English Comments
Dielectric Strength 20.3 kV/mm

@Thickness 3.20 mm
516 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Dielectric Strength 20.3 kV/mm

@Thickness 3.20 mm
516 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Dielectric Strength 20.3 kV/mm

@Thickness 3.20 mm
516 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Dielectric Strength 20.3 kV/mm

@Thickness 3.20 mm
516 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Dielectric Strength 20.3 kV/mm

@Thickness 1.91 mm
516 kV/in

@Thickness 0.0750 in
Momentive Performance Materials RTV11 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Dielectric Strength 20.3 kV/mm

@Thickness 1.90 mm
516 kV/in

@Thickness 0.0748 in
Momentive Performance Materials RTV41 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Dielectric Strength 20.3 kV/mm

@Thickness 1.91 mm
516 kV/in

@Thickness 0.0750 in
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Dielectric Strength 20.3 kV/mm

@Thickness 3.20 mm
516 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® HPH4504H PPC
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..