Electrical Properties Metric English Comments
Dielectric Strength 190 kV/mm

@Temperature 23.0 °C
4830 kV/in

@Temperature 73.4 °F
1/4 inch electrode; ASTM D149
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline
APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI..
Dielectric Strength 190 kV/mm
4830 kV/in
MD, 6.25mm (0.25in) electrode; ASTM D149
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..
Dielectric Strength 190 kV/mm
4830 kV/in
TD, 6.25mm (0.25in) electrode; ASTM D149
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..
Dielectric Strength 190 kV/mm

@Temperature 23.0 °C
4830 kV/in

@Temperature 73.4 °F
1/4 inch electrode; ASTM D149
Victrex® APTIV® 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous
APTIV PEEK 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK ..
Dielectric Strength 190 kV/mm

@Thickness 0.0250 mm
4830 kV/in

@Thickness 0.000984 in
ASTM D149
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU)
Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU ..
Dielectric Strength 190 kV/mm
4830 kV/in
MD, 6.25mm (0.25in) electrode; ASTM D149
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..
Dielectric Strength 190 kV/mm
4830 kV/in
TD, 6.25mm (0.25in) electrode; ASTM D149
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..