Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.2 kV/mm | 462 kV/in | Short Time; ASTM D149 |
Plenco 50030 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Dielectric Strength | 18.2 kV/mm | 462 kV/in | ASTM D149 |
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t.. |