Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.0 - 18.0 kV/mm | 254 - 457 kV/in | Average value: 14.7 kV/mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 16.0 - 18.0 kV/mm | 406 - 457 kV/in | Average value: 16.6 kV/mm Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 16.5 - 18.0 kV/mm | 420 - 457 kV/in | Average value: 17.6 kV/mm Grade Count:4 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |