Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 43.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 43.3 kV/mm
1100 kV/in
IPC-TM-650.2.5.6.2
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy
The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f..
Dielectric Strength 43.3 - 51.2 kV/mm
1100 - 1300 kV/in
ASTM D149
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Dielectric Strength 43.3 kV/mm
1100 kV/in
ASTM D149
Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported)
Design/Construction:Material: Cured Silicone RubberLiner: Polyethylene Recommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicon..
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 941 Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9461P Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9461PC Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 965 Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 966 Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Dielectric Strength 43.3 kV/mm
1100 kV/in
IPC TM-650 2.5.6.2
Arlon CLTE Microwave Printed Circuit Board Substrate
CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/..
Dielectric Strength 43.3 kV/mm
1100 kV/in
ASTM D149
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d..
Dielectric Strength 43.3 kV/mm
1100 kV/in
12 to 15 mil coating; ASTM D149
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var..
Dielectric Strength 43.3 kV/mm
1100 kV/in
ASTM D257
3M Scotch-Weld™ DP-100NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M
Dielectric Strength 43.3 kV/mm
1100 kV/in
ASTM D149
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Dielectric Strength 43.3 - 51.2 kV/mm
1100 - 1300 kV/in
ASTM D149
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Dielectric Strength 43.3 kV/mm
1100 kV/in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
3M 9462P Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Dielectric Strength 43.3 kV/mm
1100 kV/in
Aremco Aremco-Bond™ 2320 High Performance Epoxide
Toughened, Unfilled, Fast-Setting, BPA Free, 2:1, High Peel & Shear Strength
Dielectric Strength 43.3 kV/mm
1100 kV/in
IPC-TM-650.2.5.6.2
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy
The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW..
Dielectric Strength 43.3 - 51.2 kV/mm
1100 - 1300 kV/in
ASTM D149
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved