Electrical Properties Metric English Comments
Dielectric Strength 42.5 kV/mm
1080 kV/in
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay..