Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.8 kV/mm | 884 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber PA 66, injection molding 30% glass fibers, UL 94 V-0 at 0.4 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, free from halogen and red phosphorous |
|||
Dielectric Strength | 34.8 kV/mm | 885 kV/in | Arlon SQA-TMS-020 |
Arlon 910-10Rxx-P1 0.010" Cured, Self-Fusing Silicone Rubber 1.0 inch wide, 0.010" thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Dielectric Strength | 34.8 kV/mm | 885 kV/in | ASTM D149 |
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |