Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.9 kV/mm @Thickness 1.60 mm |
861 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |
|||
Dielectric Strength | 33.9 kV/mm | 860 kV/in | ASTM D149 |
Loctite® Shadowcure™ 397 Acrylic/urethane Heat Cure Coating Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti.. |
|||
Dielectric Strength | 33.9 kV/mm | 860 kV/in | |
Aremco Aremco-Bond™ 820 High Performance Epoxide Clear, 1:1, 45-Minute Cure System with Good Flexibility |
|||
Dielectric Strength | 33.9 kV/mm | 860 kV/in | ASTM D257 |
3M Scotch-Weld™ DP-100 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP-100 is a two-part adhesives offering fast cure and machinability.Information provided by 3M |