Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 33.0 kV/mm | 838 kV/in | STN IEC 60243 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Lanxess Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral PET + PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | ASTM D149 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A1030FR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | cond; IEC 60243-1 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15 Information provided by EMS Grivory |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4129 black 9020 PA610 Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high res.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | ASTM D149, IEC 243 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65 Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30 Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | CEI 60243-1 |
Addiplast Addinyl B2 ZV20 Nylon 6, 20% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | IEC 60243-1 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | CEI 60243-1 |
Addiplast Addinyl B2 G10 V20 Nylon 6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Dielectric Strength | 33.0 kV/mm @Thickness 2.00 mm |
838 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Dielectric Strength | 33.0 kV/mm | 838 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |